Inconel 600 hexagonal hole perforated sheet is stocked to DIN 24041 (Hv). The alloy provides excellent oxidation resistance at extreme temperature and is essentially non-magnetic; the practical service limit is approx. +1000 °C (short excursions higher). Property data, alloy comparison and the specification table follow.
Why Choose Inconel 600 for Hexagonal Hole Perforated Sheet
The high-temperature furnace and hot-gas filtration alloy. For hexagonal hole perforated sheet, this matters when excellent oxidation resistance at extreme temperature is the controlling requirement.
Alloy Properties
| Grade designation | UNS N06600 (2.4816) |
|---|---|
| Magnetic response | Essentially non-magnetic |
| Service temperature | approx. +1000 °C (short excursions higher) |
| Corrosion characteristic | Excellent oxidation resistance at extreme temperature |
Corrosion Behavior in Filtration Service
Nickel-family alloys are specified for hexagonal hole perforated sheet when stainless is not enough: Monel 400 for seawater and hydrofluoric acid, Inconel 600 for oxidation at extreme temperature, Hastelloy C-276 for hot chlorides and mixed acids, titanium for chlorides with weight savings. Match the alloy to the specific chemistry — they are not interchangeable.
Cleaning & Compatibility
Special alloys tolerate aggressive cleaning chemistry, but confirm the specific acid/alkali against the alloy datasheet — e.g. Monel handles HF but not oxidizing nitric; titanium handles nitric but not HF. When welding elements into frames, use matching filler and inert-gas backing to preserve corrosion resistance at the joint.
Specifications of Hexagonal Hole Perforated Sheet Available in Inconel 600
| Across flats (mm) | Pitch (mm) | Open area (%) | Thickness (mm) | Reference standard |
|---|---|---|---|---|
| 3.0 | 4.0 | 51 | 1.0 | DIN 24041 |
| 5.0 | 6.5 | 54 | 1.5 | DIN 24041 |
| 8.0 | 10.0 | 58 | 2.0 | DIN 24041 |
| 10.0 | 12.5 | 58 | 2.0 | DIN 24041 |
| 15.0 | 18.0 | 63 | 3.0 | DIN 24041 |