Material page for five-heddle weave mesh in Inconel 600. The high-temperature furnace and hot-gas filtration alloy. Covers the grade designation (UNS N06600 (2.4816)), corrosion and magnetic behavior, cleaning and compatibility notes, and the specifications available.
Why Choose Inconel 600 for Five-Heddle Weave Mesh
The high-temperature furnace and hot-gas filtration alloy. For five-heddle weave mesh, this matters when excellent oxidation resistance at extreme temperature is the controlling requirement.
Alloy Properties
| Grade designation | UNS N06600 (2.4816) |
|---|---|
| Magnetic response | Essentially non-magnetic |
| Service temperature | approx. +1000 °C (short excursions higher) |
| Corrosion characteristic | Excellent oxidation resistance at extreme temperature |
Corrosion Behavior in Filtration Service
Nickel-family alloys are specified for five-heddle weave mesh when stainless is not enough: Monel 400 for seawater and hydrofluoric acid, Inconel 600 for oxidation at extreme temperature, Hastelloy C-276 for hot chlorides and mixed acids, titanium for chlorides with weight savings. Match the alloy to the specific chemistry — they are not interchangeable.
Cleaning & Compatibility
Special alloys tolerate aggressive cleaning chemistry, but confirm the specific acid/alkali against the alloy datasheet — e.g. Monel handles HF but not oxidizing nitric; titanium handles nitric but not HF. When welding elements into frames, use matching filler and inert-gas backing to preserve corrosion resistance at the joint.
Specifications of Five-Heddle Weave Mesh Available in Inconel 600
| Mesh (warp x weft) | Warp wire (mm) | Weft wire (mm) | Nominal filtration (u00b5m) | Weight SS (kg/mu00b2) | Reference standard |
|---|---|---|---|---|---|
| 30x360 | 0.25 | 0.16 | 80 | 1.15 | ISO 9044 |
| 40x560 | 0.18 | 0.12 | 60 | 0.90 | ISO 9044 |
| 80x720 | 0.10 | 0.07 | 32 | 0.55 | ISO 9044 |